ABSTRACT
Polycrystalline silicon-gate metal-oxide-semiconductor (MOS) capacitors have been fabricated with high-temperature anneals from 800 to 950 °C after gate oxidation and polycrystalline silicon deposition. Temperatures from 800 to 875 °C are found to have very little effect on the radiation response of these devices. However, a rapid increase in radiation-induced oxide-trapped charge, ΔVot, is observed for anneal temperatures above 875 °C. This increase in ΔVot coincides with an experimentally observed change in the polycrystalline silicon grain structure. The anneal temperature was found to have a much smaller effect on radiation-induced interface-trap charge. The correlation of these results to other properties, e.g., stress, is discussed.
ACCESSION #
9827894

 

Related Articles

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics