ABSTRACT
Ga-As-In-As superalloy has been grown by atomic epitaxy on InP substrates. This has been achieved by sequential exposure of the substrate to trimethylgallium, arsine, triethylindium, and arsine. The thickness of the deposited film is in excellent agreement with the predicted value based on the number of exposure cycles. These results demonstrate that atomic layer epitaxy offers the ultimate control for depositing thin films. The superalloy films have been characterized by transmission electron microscopy and photoluminescence.
ACCESSION #
9825093

 

Related Articles

  • Maskless growth of InP stripes on patterned Si (001): Defect reduction and improvement of.... Grundmann, M.; Krost, A. // Applied Physics Letters;6/29/1992, Vol. 60 Issue 26, p3292 

    Investigates the metalorganic vapor phase epitaxy of indium phosphide stripes on narrow silicon stripes. Occurrence of complete suppression of antiphase domains; Location of the termination of the stacking faults; Achievement of smoother surface morphology and increased quantum efficiency.

  • Use of triethylindium and bisphosphinoethane for the growth on InP by chemical beam epitaxy. Chin, Albert; Martin, Paul; Das, Utpal; Mazurowski, John; Ballingall, Jim // Applied Physics Letters;10/26/1992, Vol. 61 Issue 17, p2099 

    Examines the chemical beam epitaxial growth of indium phosphide using bisphosphinoethane as a group V source. Observation of a mirrorlike surface morphology and excellent reflection high-energy electron diffraction patterns; Measurement of the linewidth of the dominant donor bound exciton;...

  • Planar regrowth of InP and InGaAs around reactive ion etched mesas using atmospheric pressure.... Lee, B.-T.; Logan, R.A. // Applied Physics Letters;7/12/1993, Vol. 63 Issue 2, p234 

    Examines the planar regrowth of indium phosphide (InP) and indium aluminum arsenide (AlGaAs) around reactive ion etched mesas using atmospheric pressure metalorganic vapor phase epitaxy. Addition of trichloroethane to InP layers; Absence of growth interruption in InP and AlGaAs layers;...

  • Kinetically controlled order/disorder structure in GaInP. Su, L.C.; Ho, I.H. // Applied Physics Letters;8/8/1994, Vol. 65 Issue 6, p749 

    Describes the organometallic vapor phase epitaxy growth of an order/disorder gallium indium phosphide heterostructure. Band-gap energy difference of the heterostructure; Composition and lattice match of the two layers; Observation on the antiphase boundaries; Details of the photoluminescence...

  • Electron beam induced current and cathodoluminescence study of the recombination activity of stacking faults and hillocks in hydride vapor phase epitaxy InP. Attolini, G.; Frigeri, C.; Pelosi, C.; Salviati, G. // Applied Physics Letters;7/21/1986, Vol. 49 Issue 3, p167 

    Cathodoluminescence and electron beam induced current modes in the scanning electron microscope have been employed to study the recombination behavior of stacking faults and surrounding hillocks in undoped InP homoepitaxies grown by hydride vapor phase epitaxy. Stacking faults exhibited...

  • Vapor phase epitaxy of InP using flow modulation. Wang, P. J.; Wessels, B. W. // Applied Physics Letters;9/8/1986, Vol. 49 Issue 10, p564 

    We report the first preparation of indium phosphide using flow modulation techniques in the hydride vapor phase epitaxial system. A conventional single barrel reactor was used. Layer growth rates as low as 25 Ã…/cycle were demonstrated. Room-temperature carrier concentrations for the...

  • Growth of In0.53Ga0.47As by liquid phase epitaxy over tungsten on structured InP substrates. Hancox, J. E.; Houston, P. A.; Hill, G.; Chand, N. // Applied Physics Letters;11/24/1986, Vol. 49 Issue 21, p1462 

    A first study involving lateral growth of In0.53Ga0.47As by liquid phase epitaxy over tungsten metal is being reported. Because of the rapid lateral nucleation process in the channels etched on (111) B InP substrates, seeding of the crystal through the metal layer is found unnecessary, enabling...

  • Growth of indium phosphide by metalorganic vapor phase epitaxy using dimethyl (3-dimethylaminopropyl) indium as a new indium source. Molassioti, A.; Moser, M.; Stapor, A.; Scholz, F.; Hostalek, M.; Pohl, L. // Applied Physics Letters;2/27/1989, Vol. 54 Issue 9, p857 

    Dimethyl (3-dimethylaminopropyl) indium was synthesized and used for the first time as an indium source for the growth of InP layers by metalorganic vapor phase epitaxy at atmospheric pressure. This compound is liquid at room temperature with a vapor pressure of 30–40 Pa at 30 °C,...

  • Determination of defect density in ZnCdMgSe layers grown on InP using chemical etch. Zeng, L.; Yang, B.X.; Shewareged, B.; Tamargo, M. C.; Wan, J. Z.; Pollak, Fred H.; Snoeks, E.; Zhao, L. // Journal of Applied Physics;10/1/1997, Vol. 82 Issue 7, p3306 

    Discusses the characterization of ZnCdMgSe epitaxial layers grown on indium phosphide substrates. Measurements of etch pit density; Characterization of the morphology of the etched surface using atomic force microscopy; Accuracy of the etch pit density method for revealing stacking faults and...

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics