TITLE

CALCULATION OF MODE PARAMETERS OF WALL BEAD DEPOSITION IN DOWNHAND MULTI-PASS GAS-SHIELDED WELDING

AUTHOR(S)
SHOLOKHOV, M. A.; BUZORINA, D. S.
PUB. DATE
July 2013
SOURCE
Paton Welding Journal;Jul2013, Issue 7, p61
SOURCE TYPE
Trade Publication
DOC. TYPE
Article
ABSTRACT
Application of narrowed grooves is an effective method to increase welding process efficiency at simultaneous reduction of financial and energy expenses. One of the main difficulties in implementation of multi-pass welding technology 10 mm thick rolled metal structures using automated and robotized units is a high possibility of defect formation such as lack of penetration, in particular, in layer of the first pass (wall bead). Control of welding parameters determining heat input is one of the methods of penetration regulation. Dependencies between welding parameters in problem areas of the grooves and penetration depth were determined experimentally. On their basis the equations for determination of parameters of bead deposition at given coefficient of areas were obtained. These results became a part of algorithm development to control welding mode parameters in automated and robotized units.
ACCESSION #
91922545

 

Related Articles

  • Effect of Thickness Ratio on Formability of Tailor Welded Blanks (TWB). Bhaskar, V. Vijay; Narayanan, R. Ganesh; Narasimhan, K.; Ghosh, S.; Castro, J. C.; Lee, J. K. // AIP Conference Proceedings;2004, Vol. 712 Issue 1, p863 

    Tailor welded blanks (TWBs) are made by welding same or different materials having same/different properties into a single blank. They can be tailored to any specific shape and size. The formability of these blanks depend on material and geometric parameters like strength ratio and thickness...

  • Stabilizer Fillet Weld Strength under Multiaxial Loading (Effect of Force, Size and Residual Stress). Hadipour, Iman; Marzbanrad, Javad // International Journal of Electrical, Computer & Systems Engineer;2007, Vol. 1 Issue 4, p234 

    In this paper, the strength of a stabilizer is determined when the static and fatigue multi-axial loading are applied. Stabilizer is a part of suspension system in the heavy truck for stabilizing the cabin against the vibration of the road which composes of a thin-walled tube joined to a forge...

  • THE EXPERIMENTAL INVESTIGATIONS OF RESIDUAL STRESSES IN TUBE WITH THICK WALLS. ATANASTU, Costica; VLASCEANU, Daniel; TRIPA, Pavel; ROSCA, Valcu; PROCA, Victor // Annals of DAAAM & Proceedings;Jan2009, p1163 

    In this paper the residual stresses produced in the welding seam from the tube with thick walls are experimental determined. After welding processes, in the welding seam appears residual stresses which can lead on the failure on the structure. The experimental determination it was made on the...

  • Defining a Critical Weld Dilution to Avoid Solidification Cracking in Aluminum. Coniglio, N.; Cross, C. E.; Michael, T.; Lammers, M. // Welding Journal;Sep2008, Vol. 87 Issue 9, p237s 

    The article discusses a study which examines the relationship between filler metal dilution, local strain rate conditions and cracking susceptibility in aluminum welds. Using the controlled tensile weldability test and local strain extensometer measurements, a boundary was established between...

  • The Tensile and Shear Strength of a Base Metal Weld Joint Used in Dentistry. MacENTEE, M. I.; HAWBOLT, E. B.; ZAHEL, J. I. // Journal of Dental Research;Feb1981, Vol. 60 Issue 2, p154 

    Samples of a base metal alloy were cast and welded together using a conventional welding procedure. The joints were loaded and placed either in a corrosive environment or in air for varying time periods. The tensile and shear strength of the joints was unaffected by the corrosive environment,...

  • 3D Thermo-Visco Plastic Analysis of Thin Shells Buckling Behavior Due to Welding. Ziaee, S.; Kadivar, M. H. // International Journal of Mechanics & Solids; 

    Welding induces residual stresses in structures which may cause buckling distortion, if they exceed the critical buckling stress of the structure. This paper presents a predictive distortion analysis approach for welded structure. 3-D thermo-mechanical welding process simulations are performed...

  • Metallic glasses: Must shear bands be hot? Spaepen, Frans // Nature Materials;Jan2006, Vol. 5 Issue 1, p7 

    The article discusses the mechanical properties of metallic glasses. A metallic glass is produced by cooling an alloy melt under conditions that prevent crystallization. Yet, the material is said to deform. In the plastic deformation of metals at low temperatures, the smaller the crystals that...

  • Metallography of Sub-Surface Flows Generated by Shock-Induced Friction. Winter, R. E.; Smeeton, V. S.; De'Ath, J.; Taylor, P.; Markland, L.; Barlow, A. J. // AIP Conference Proceedings;2004, Vol. 706 Issue 1, p625 

    A configuration is described in which an explosively-generated shock is driven obliquely across the interface between aluminium and steel anvils causing them to slide against each other. The interface pressures and the time at which the surfaces separate, are estimated using hydro-code...

  • The mechanism of hydrogen embrittlement: the stress interaction between a crack, a hydrogen cluster, and moving dislocations. Yokobori Jr., A.T. // International Journal of Fracture;Jul/Aug2004, Vol. 128 Issue 1-4, p121 

    Mechanisms of dissolvent anodic chemical reaction and hydrogen embrittlement have been proposed as stress corrosion cracking (SCC) mechanisms. The former is feasible for the case of plastic deformation dominant metals (low-yield stress), and the latter is for high-strength metals such as...

Share