TITLE

Enthalpy relaxation of homogeneous polystyrene/poly(2-chloro styrene) blends measured by differential scanning calorimetry

AUTHOR(S)
Takahashi, Masato; Orino, Daisuke; Saito, Masahito; Kobayashi, Hideyuki; Kajiwara, Kanji; Matsuda, Hideomi
PUB. DATE
June 2000
SOURCE
AIP Conference Proceedings;2000, Vol. 519 Issue 1, p199
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
© 2000 American Institute of Physics.
ACCESSION #
5665071

 

Related Articles

  • Heterogeneous dynamics, ageing, and rejuvenating in van der Waals liquids. Merabia, Samy; Long, Didier // Journal of Chemical Physics;12/21/2006, Vol. 125 Issue 23, p234901 

    It has been shown over the past ten years that the dynamics close to the glass transition is strongly heterogeneous: fast domains coexist with domains three or four decades slower, the size of these regions being about 3 nm at Tg. The authors extend here a model that has been proposed recently...

  • Temperature scanning small angle x-ray scattering measurements of structural relaxation in type-III vitreous silica. Brüning, R.; Levelut, C.; Le Parc, R.; Faivre, A.; Semple, L.; Vallee, M.; Simon, J.-P.; Hazemann, J.-L. // Journal of Applied Physics;Oct2007, Vol. 102 Issue 8, p083535 

    The fictive temperature of vitreous silica containing approximately 900 wt ppm of hydroxyl groups was monitored with small angle x-ray scattering. The measurements were carried out during annealing and while scanning the temperature, with annealing temperatures ranging between 930 and 1330 K....

  • Energy relaxation and dephasing dynamics of colored filter glasses. Nakano, H.; Ishida, Y.; Yanagawa, T. // Applied Physics Letters;12/9/1991, Vol. 59 Issue 24, p3090 

    Measures the relaxation and dephasing time constants of colored filter glasses. Influence of the photodarkening effect on the relaxation time; Role of irradiation in nonlinearity changes of the colored glass; Occurrence of the dephasing process.

  • Low-temperature dielectric behavior of Nb[sub 2]O[sub 5]–SiO[sub 2] solid solutions. Choosuwan, H.; Guo, R.; Bhalla, A. S.; Balachandran, U. // Journal of Applied Physics;3/1/2003, Vol. 93 Issue 5, p2876 

    Dielectric properties of Nb[sub 2]O[sub 5](0.92):SiO[sub 2](0.08) ceramic were measured in the temperature range of 10-300 K by the cryostat system. Frequency-dependent dielectric loss suggests the relaxation behavior of this material. The relaxation mechanism was analyzed by the Arrhenius...

  • Critical fluctuations and relaxation phenomena in the isotopic blend polystyrene/deuteropolystyrene investigated by small angle neutron scattering. Schwahn, D.; Hahn, K.; Streib, J.; Springer, T. // Journal of Chemical Physics;12/1/1990, Vol. 93 Issue 11, p8383 

    For the isotopic blend of polystyrene (PS) PS/deutero PS (M=106 dalton), the Flory–Huggins interaction parameter χ([lowercase_phi_synonym],T) was determined by means of the structure factor S(Q) measured by small angle neutron scattering (SANS). From χ([lowercase_phi_synonym],T),...

  • Macroscopic facilitation of glassy relaxation kinetics: Ultrastable glass films with frontlike thermal response. Léonard, Sébastien; Harrowell, Peter // Journal of Chemical Physics;12/28/2010, Vol. 133 Issue 24, p244502 

    The recent experimental fabrication of ultrastable glass films, via vapor deposition [Swallen et al., Science 315, 353 (2007)] and the observation of frontlike response to the annealing of these films [Swallen et al., Phys. Rev. Lett. 102, 065503 (2009)] have raised important questions about the...

  • Physical aging in a hyperquenched glass. Yue, Y. Z.; Jensen, S. L.; deC. Christiansen, J. // Applied Physics Letters;10/14/2002, Vol. 81 Issue 16, p2983 

    We report experimental data on the enthalpy relaxation of a hyperquenched silicate glass subjected to long-time aging (annealing) below the glass-transition temperature (T[sub g]). The relaxation of a hyperquenched glass substantially differs from that of a normally cooled glass. Two mechanisms...

  • Dynamic model for pseudomorphic structures grown on compliant substrates: An approach to extend.... Teng, D.; Lo, Y.H. // Applied Physics Letters;1/4/1993, Vol. 62 Issue 1, p43 

    Develops a dynamic model to analyze the critical thickness for pseudomorphic structures grown on thin membranes. Consideration of the strain relaxation process; Result of analysis on gallium arsenide/indium gallium arsenide material system; Fabrication of semiconductor lasers with yellow and...

  • Structural relaxation of an unentangled polymer in terms of a simple phenomenological approach. Andreozzi, Laura; Autiero, Ciro; Faetti, Massimo; Zulli, Fabio // Journal of Chemical Physics;8/28/2007, Vol. 127 Issue 8, p084909 

    The enthalpy relaxation mechanism of a low molecular weight synthesis of polymethylmethacrylate was investigated by means of calorimetric experiments. The data were analyzed in terms of a kinetic approach treating nonlinearity in a different manner with respect to the Tool-Narayanaswamy-Moynihan...

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics