The influences of surface treatment and gas annealing conditions on the inversion behaviors of the atomic-layer-deposition Al2O3/n-In0.53Ga0.47As metal-oxide-semiconductor capacitor

Trinh, H. D.; Chang, E. Y.; Wu, P. W.; Wong, Y. Y.; Chang, C. T.; Hsieh, Y. F.; Yu, C. C.; Nguyen, H. Q.; Lin, Y. C.; Lin, K. L.; Hudait, M. K.
July 2010
Applied Physics Letters;7/26/2010, Vol. 97 Issue 4, p042903
Academic Journal
The inversion behaviors of atomic-layer-deposition Al2O3/n-In0.53Ga0.47As metal-oxide-semiconductor capacitors are studied by various surface treatments and postdeposition annealing using different gases. By using the combination of wet sulfide and dry trimethyl aluminum surface treatment along with pure hydrogen annealing, a strong inversion capacitance-voltage (C-V) response is observed, indicating a remarkable reduction in interface trap state density (Dit) at lower half-part of In0.53Ga0.47As band gap. This low Dit was confirmed by the temperature independent C-V stretch-out and horizontal C-V curves. The x-ray photoelectron spectroscopy spectra further confirm the effectiveness of hydrogen annealing on the reduction of native oxides.


Related Articles

  • Band Offsets in the Mg0.5Ca0.5O/GaN Heterostructure System. Chen, J.-J.; Hlad, M.; Gerger, A. P.; Gila, B. P.; Ren, F.; Abernathy, C. R.; Pearton, S. J. // Journal of Electronic Materials;Apr2007, Vol. 36 Issue 4, p368 

    MgCaO offers promise as a gate dielectric for GaN-based metal-oxide-semiconductor (MOS) transistors, particularly in combination with environmentally stable capping layers such as Sc2O3. X-ray photoelectron spectroscopy (XPS) was used to measure the energy discontinuity in the valence band...

  • Compositional dependencies of ferromagnetic Ge1-xMnxTe grown by solid-source molecular-beam epitaxy. Chen, W. Q.; Teo, K. L.; Jalil, M. B. A.; Liew, T. // Journal of Applied Physics;4/15/2006, Vol. 99 Issue 8, p08D515 

    The IV-VI diluted magnetic semiconductor Ge1-xMnxTe thin films on BaF2 (111) substrate have been prepared using solid-source molecular-beam epitaxy technique by varying the Mn concentrations from x=0.25 to 0.98. The chemical Mn concentration was determined by x-ray photoelectron spectroscopy...

  • Ultralow equivalent oxide thickness obtained for thin amorphous LaAlO3 layers grown on Si(001). Becerra, L.; Merckling, C.; Baboux, N.; Plossu, C.; Marty, O.; El-Kazzi, M.; Saint-Girons, G.; Vilquin, B.; Hollinger, G. // Applied Physics Letters;11/5/2007, Vol. 91 Issue 19, p192909 

    Electron beam evaporation in a molecular beam epitaxy reactor was used to deposit, at 400 °C, amorphous LaAlO3 high-κ oxide films on p-type Si(001). X-ray photoelectron spectroscopy and transmission electron microscopy showed that the interface with Si is free of SiO2 or silicates....

  • Bi-induced acceptor states in ZnO by molecular-beam epitaxy. Xiu, F. X.; Mandalapu, L. J.; Yang, Z.; Liu, J. L.; Liu, G. F.; Yarmoff, J. A. // Applied Physics Letters;7/31/2006, Vol. 89 Issue 5, p052103 

    Bi-doped ZnO films were grown on Si (111) substrates by molecular-beam epitaxy. X-ray photoelectron spectroscopy and diffraction measurements reveal that Bi was incorporated into ZnO films without any phase separation. Room-temperature Hall effect measurements show a significant reduction of...

  • Growth and strain compensation effects in the ternary Si[sub 1-x-y]Ge[sub x]C[sub y] alloy system. Eberl, K.; Iyer, S.S. // Applied Physics Letters;6/15/1992, Vol. 60 Issue 24, p3033 

    Reports the synthesis of pseudomorphic Si[sub 1-y]C[sub y] and Si[sub 1-x-y]Ge[sub x]C[sub y] alloy layers on a silicon substrate by molecular beam epitaxy using solid sources. Importance of strain compensation in heterostructure engineering; Effect of the pseudomorphic composition on the...

  • Compositional variation of nearly lattice-matched InAlGaN alloys for high electron mobility transistors. Lim, T.; Aidam, R.; Kirste, L.; Waltereit, P.; Quay, R.; Müller, S.; Ambacher, O. // Applied Physics Letters;6/21/2010, Vol. 96 Issue 25, p252108 

    Quaternary InAlGaN semiconductors with AlN mole fractions between 40% and 81% and respective InN contents of 7% and 19% including InAlN as a ternary border case have been grown by plasma-assisted molecular beam epitaxy. The electron mobility in InAlGaN-based heterostructures increases with Ga...

  • Optical Characteristics of ZnTeO Thin Films Synthesized by Pulsed Laser Deposition and Molecular Beam Epitaxy. Wang, W.; Bowen, W.; Spanninga, S.; Lin, S.; Phillips, J. // Journal of Electronic Materials;Jan2009, Vol. 38 Issue 1, p119 

    Oxygen incorporation into ZnTe was studied using pulsed laser deposition and molecular beam epitaxy. Oxygen incorporation at the high partial pressures studied for pulsed laser deposition was found to result in increasing visible transparency with oxygen incorporation, and is attributed to the...

  • Application of Zn-contaminated soil: Feasibility study on the removal of HS from hot coal-derived gas. Tzu-Hsing Ko // Environmental Chemistry Letters;Mar2011, Vol. 9 Issue 1, p77 

    In this study, zinc-contaminated soils were chosen as a candidate material for the removal of hydrogen sulfide (HS) from hot coal-derived gas. Laboratory experiments showed that HS was decreased to less than 10 ppm when the zinc-contaminated soils were reacted with HS. The best removal...

  • Optimum growth condition of single-crystalline undoped ZnS grown by the molecular-beam-epitaxial method using a H2S gas source. Kaneda, Shigeo; Shimoguchi, Takefumi; Takahashi, Hironobu; Motoyama, Shin-ici; Kano, Fumihisa; Yokoyama, Meiso; Satou, Shuji // Journal of Applied Physics;10/15/1988, Vol. 64 Issue 8, p3945 

    Presents a study that investigated the optimum growth condition of single-crystalline undoped zinc sulphide grown by the molecular-beam-epitaxial method using a hydrogen sulphide gas source. Details of the experiment; Conclusions.