TITLE

Epitaxial growth of Ba[sub 1-x]K[sub x]BiO[sub 3] thin films by pulsed-laser deposition

AUTHOR(S)
Norton, D.P.; Budai, J.D.; Chakoumakos, B.C.; Feenstra, R.
PUB. DATE
January 1993
SOURCE
Applied Physics Letters;1/25/1993, Vol. 62 Issue 4, p414
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
Examines the epitaxial growth of Ba[sub 1-x]K[sub x]BiO[sub 3] thin films by pulsed-laser deposition. Orientation of the epitaxial films; Use of x-ray diffraction to assess crystal structures; Determination of optimal growth temperature.
ACCESSION #
4329501

 

Related Articles

  • Epitaxial growth by pulsed laser deposition of Er-doped Sc2O3 films on sesquioxides monitored in situ by reflection high energy electron diffraction. Gün, Teoman; Kuzminykh, Yury; Petermann, Klaus; Scheife, Hanno; Huber, Günter // Applied Physics Letters;8/20/2007, Vol. 91 Issue 8, p083103 

    In this letter, the authors report on the epitaxial growth by pulsed laser deposition of Sc2O3 and Er(5%):Sc2O3 films on {100} and {111} oriented Sc2O3. They observed layer-by-layer growth in the orientation defined by the substrate. This was indicated by reflection high energy electron...

  • Epitaxial growth of non-c-oriented ferroelectric SrBi[sub 2] Ta[sub 2] O[sub 9] thin films on Si(100) substrates. Lee, H.N.; Senz, S.; Visinoiu, A.; Pignolet, A.; Hesse, D.; Gösele, U. // Applied Physics A: Materials Science & Processing;2000, Vol. 71 Issue 1, p101 

    Abstract. Epitaxial SrBi[sub 2]Ta[sub 2]O[sub 9] (SBT) thin films with well-defined (116) orientation have been grown by pulsed laser deposition on Si(100) substrates covered with an yttriastabilized ZrO[sub 2] (YSZ) buffer layer and an epitaxial layer of electrically conductive SrRuO[sub 3]....

  • Phase transitions in epitaxial Ba0.5Sr0.5TiO3 thin films. Ríos, S.; Scott, J. F.; Lookman, A.; McAneney, J.; Bowman, R. M.; Gregg, J. M. // Journal of Applied Physics;1/15/2006, Vol. 99 Issue 2, p024107 

    Ba0.5Sr0.5TiO3 (BST) thin-film capacitor structures with various thicknesses, (50–1200 nm) and different strain conditions (on lanthanum strontium cobalt oxide La0.5Sr0.5CoO3 and strontium ruthenate SrRuO3 buffer layers) were made using pulsed laser deposition, and characterized by x-ray...

  • Thermally driven solid-phase epitaxy of laser-ablated amorphous AlFe films on (0001)-oriented sapphire single crystals. Trautvetter, Moritz; Wiedwald, Ulf; Paul, Heiko; Minkow, Alexander; Ziemann, Paul // Applied Physics A: Materials Science & Processing;Mar2011, Vol. 102 Issue 3, p725 

    Solid-phase epitaxy is demonstrated for the metallic binary alloy AlFe. Stoichiometric thin films are deposited at ambient temperature onto c-cut sapphire by pulsed laser deposition (PLD), resulting in smooth amorphous films as revealed by X-ray diffraction (XRD) and atomic force microscopy...

  • Critical factor for epitaxial growth of cobalt-doped BaFe2As2 films by pulsed laser deposition. Hidenori Hiramatsu; Hikaru Sato; Takayoshi Katase; Toshio Kamiya; Hideo Hosono // Applied Physics Letters;4/28/2014, Vol. 104 Issue 17, p1 

    We heteroepitaxially grew cobalt-doped BaFe2As2 films on (La,Sr)(Al,Ta)O3 single-crystal substrates by pulsed laser deposition using four different wavelengths and investigated how the excitation wavelength and pulse energy affected growth. Using the tilting and twisting angles of X-ray...

  • Influence of CeO-Cap Layer on the Texture and Critical Current Density of YBCO Film. Xu, Da; Liu, Linfei; Wang, Ying; Zhu, Shengping; Zhu, Peng; Li, Yijie // Journal of Superconductivity & Novel Magnetism;Apr2012, Vol. 25 Issue 2, p197 

    YBaCuO (YBCO) thin films have been fabricated on different textured CeO-cap layers by pulsed laser deposition (PLD). The texture and critical current density J of YBCO thin films have been systematically investigated. Both in-plane and out-of-plane textures of YBCO films and CeO-cap films were...

  • Chirally oriented heteroepitaxial thin films grown by pulsed laser deposition: Pt(621) on SrTiO3(621). Francis, Andrew J.; Salvador, Paul A. // Journal of Applied Physics;9/1/2004, Vol. 96 Issue 5, p2482 

    Pulsed laser deposition has been used to grow Pt(621) thin films having a chiral orientation on SrTiO3(621) substrates. Films were deposited over a range of conditions, then characterized for their crystallinity and epitaxy using x-ray diffraction and for their surface morphologies using atomic...

  • Superconducting and structural properties of in-plane aligned a-xis oriented.... Gun Yong Sung; Jeong Dae Suh // Applied Physics Letters;8/21/1995, Vol. 67 Issue 8, p1145 

    Examines the superconducting and structural properties of YBa[sub 2]Cu[sub 3]O[sub 7-x] (YBCO) thin films. Use of x-ray diffraction analysis to determine the in-plane alignment of YBCO layers; Effect of deposition temperature on the degree of in-plane alignment; Use of pulsed laser deposition...

  • Comparative analysis of the growth of SmBa[sub 2] Cu[sub 3] O[sub 7-x] thin films by off-axis pulsed laser deposition on different substrates. Di Trolio, A.; Morone, A. // Applied Physics A: Materials Science & Processing;1999, Vol. 69 Issue 7, pS561 

    Abstract. The growth of SmBa[sub 2]Cu[sub 3]O[sub 7-x] superconducting thin films by off-axis pulsed laser deposition on different substrates (SrTiO[sub 3], MgO, LaAlO[sub 3], and YSZ) has been analyzed by means of resistance vs. temperature and X-ray diffraction measurements. The onset and...

Share

Read the Article

Courtesy of VIRGINIA BEACH PUBLIC LIBRARY AND SYSTEM

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics