TITLE

Replicated photonic crystals by atomic layer deposition within holographically defined polymer templates

AUTHOR(S)
Graugnard, E.; Roche, O. M.; Dunham, S. N.; King, J. S.; Sharp, D. N.; Denning, R. G.; Turberfield, A. J.; Summers, C. J.
PUB. DATE
June 2009
SOURCE
Applied Physics Letters;6/29/2009, Vol. 94 Issue 26, p263109
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
We report the replication of holographically defined photonic crystals using multistage atomic layer deposition. Low- and high-temperature atomic layer depositions were combined with selective etching to deposit and remove multiple conformal thin films within three-dimensional polymer templates. Using intermediate Al2O3 inverse replicas, temperature-sensitive SU-8 photonic crystal templates were faithfully replicated with TiO2 and GaP, greatly increasing the dielectric contrasts of the photonic crystals. Optical measurements are in good agreement with the calculated band structures.
ACCESSION #
42961924

 

Related Articles

Share

Read the Article

Courtesy of VIRGINIA BEACH PUBLIC LIBRARY AND SYSTEM

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics