TITLE

Differential scanning calorimetric study of hydrogen-induced amorphization in C15 Laves phase

AUTHOR(S)
Aoki, K.; Li, X-G.
PUB. DATE
November 1992
SOURCE
Applied Physics Letters;11/16/1992, Vol. 61 Issue 20, p2422
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
Examines the use of differential scanning calorimetry and x-ray diffractometry to monitor reactions of C15 Laves phase GdCo[sub 2]. Determination of reaction enthalpy change; Values of enthalpy change of hydrogen absorption, hydrogen-induced amorphization and crystallization; List of solid state amorphization reactions.
ACCESSION #
4240797

 

Related Articles

  • Al-Pt-Ti (Aluminum-Platinum-Titanium). Raghavan, V. // Journal of Phase Equilibria & Diffusion;Apr2012, Vol. 33 Issue 2, p147 

    The article offers information on the ternary system Aluminum-Platinum-Titanium (Al-Pt-Ti). It mentions the updated binary system of Al-Pt-Ti diagram which include a hexagonal type, tetragonal type, and orthorhombic. It says that based on its annealing, the compound shows its different phases...

  • Structural signature of the configurational entropy change during the glass formation of plastic crystal cyanoadamantane. Willart, J. F.; Willart, J.F.; Descamps, M.; van Miltenburg, J. C.; van Miltenburg, J.C. // Journal of Chemical Physics;6/22/2000, Vol. 112 Issue 24 

    Calorimetric and x-ray diffraction experiments are combined to characterize the entrance of a cyanoadamantane plastic crystal into a glassy crystal state upon cooling. As usually observed for glass-forming liquids, the configurational entropy of this glassy crystal is shown to strongly decrease...

  • Sodium and silver phosphate glasses doped with chlorides of Fe, Mn and Zn. Das, S. S.; Srivastava, V. // Journal of Thermal Analysis & Calorimetry;Feb2007, Vol. 87 Issue 2, p365 

    A number of samples of sodium and silver phosphate glasses doped with various compositions of some transition metals viz. iron, manganese and zinc chlorides alongwith undoped samples of sodium and silver phosphate glasses were synthesized and characterized by X-ray diffraction, IR spectral,...

  • Epitaxial growth of cubic Laves phase intermetallic compounds (YCo2, TbCo2) and new epitaxial relationship between fcc (111) and bcc (110). Robaut, F.; Jaren, S.; Cherief-Benbrahim, N.; Meyer, C. // Applied Physics Letters;9/9/1996, Vol. 69 Issue 11, p1643 

    YCo2 and TbCo2 Laves phase compounds were epitaxially grown on (110) W buffer layers by pulsed laser deposition at a base pressure of 5×10-10 Torr and a substrate temperature of 500 °C. The films were characterized in situ by reflection high-energy electron diffraction, and after...

  • Effects of heteroepitaxial strain on Laves phases TbFe, and DyFe2. Huth, M.; Flynn, C.P. // Journal of Applied Physics;6/1/1998 Part 2 of 2, Vol. 83 Issue 11, p7216 

    Investigates the structural properties of thin epitaxial tellurium and iron (TbFe)2 and dysprosium (Dy)Fe2 films grown under various conditions, focusing on the influence of structure on their magnetic properties. Reference to the cubic Laves phase compounds of the tye RFe2.

  • Magnetocaloric effect in the Laves phase pseudobinary Er[sub 1-c]Y[sub c]Co[sub 2]. de Oliveira, N. A.; von Ranke, P. J.; Costa, M. V. Tovar; Troper, A. // Journal of Applied Physics;5/15/2002 Part 1, 2 & 3, Vol. 91 Issue 10, p8879 

    In this article we study the magnetocaloric effect in the pseudobinary Er[sub 1-c]Y[sub c]Co[sub 2] using a theoretical model, in which the localized 4f spins are immersed in an effective subsystem of itinerant electrons. The interaction between the localized 4f spins is treated in the molecular...

  • Concentration and temperature dependence of electrical resistivity in Zr1-xHoxCo2 (0≤x≤1) intermetallic compounds and their hydrides. Ramesh, R.; Rama Rao, K. V. S. // Journal of Applied Physics;9/15/1994, Vol. 76 Issue 6, p3556 

    Deals with the electrical resistivity studies that have been carried out on the C 15-type Laves phase intermetallic compounds and their hydrides in the temperature range 16-300 K. Experimental details; Results and discussion; Conclusion.

  • Correlation of magneto-volume effects and local properties of the Fe2Ti-laves phase (abstract). Pelloth, J.; Brand, R. A.; Keune, W. // Journal of Applied Physics;11/15/1994, Vol. 76 Issue 10, p6912 

    Presents an abstract of the study 'Correlation of Magneto-volume Effects and Local Properties of the Fe2Ti-laves Phase,' by J. J. Pelloth, R.A. Brand and W. Keune.

  • Magnetization and magnetostriction of dendritic [112] TbxDyyHozFe1.95 (x+y+z=1) rods under... Wun-Fogle, M.; Restorff, J.B.; Clark, A.E.; Lindberg, J.F. // Journal of Applied Physics;6/1/1998 Part 2 of 2, Vol. 83 Issue 11, p7279 

    Presents a study in which the field dependencies of the magnetization and magnetostriction of the Laves phase pseudobinary TbxDyyHozFe1.95 (x+y+z=1) compounds were measured as a function of compressive stress T and applied to magnetic field H. Effects of crystalline anisotropy in the...

Share

Read the Article

Courtesy of VIRGINIA BEACH PUBLIC LIBRARY AND SYSTEM

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics