ABSTRACT
The pitting corrosion behaviour of type UNS S31603 stainless steel (316L SS) in 0.01, 0.05 and 0.1 M thiosulfate ion (S2O32-) in the absence and presence of various concentrations of chloride ion (Cl-) was studied using the cyclic potentiodynamic polarization method. The influence of major factors which affect pitting corrosion such as pH and temperature, were also investigated. It was found that both the pitting potential (Epit) and the repassivation potential (Erp) decreased with increase in Cl- concentration and solution temperature and a more pronounced difference in Epit values for various concentrations of S2O32- in 1.0 M Cl- was obtained at lower temperatures. The effect of pH on Epit, Ecorr and Erp values for different concentrations of S2O32- in the presence of 1.0 M Cl- was also determined.
ACCESSION #
16781876

 

Related Articles

  • Electrochemical characterization of AISI 316L stainless steel in contact with simulated body fluid under infection conditions. López, Danián Alejandro; Durán, Alicia; Ceré, Silvia Marcela // Journal of Materials Science: Materials in Medicine;May2008, Vol. 19 Issue 5, p2137 

    Titanium and cobalt alloys, as well as some stainless steels, are among the most frequently used materials in orthopaedic surgery. In industrialized countries, stainless steel devices are used only for temporary implants due to their lower corrosion resistance in physiologic media when compared...

  • Formation of self-organized pore arrays on metallic substrates by anodization and their applications. Hiroaki Tsuchiya // Materials Science Forum;2014, Vol. 783-786, p2034 

    The present work examines pore formation on type 316 stainless steel, Inconel 600 alloy and Co-Cr alloy. Ordered pore arrays are formed on the metallic substrates by electrochemical treatments in organic solvents containing perchlorate ions under optimized conditions. It is revealed that the Key...

  • Effect of hydrochloric acid on electrochemical behaviour of 430 stainless steel. Jiang, M. F.; Li, X. L.; Yue, Y. Y.; Shi, P. Y.; Liu, C. J. // Materials Research Innovations;Aug2014 Supplement 5, Vol. 18 Issue S5, pS62 

    The hydrochloric acid pickling process ensures high speeds with little pollution, for which a systematic study of the electrochemical behaviour of stainless steel in the oxidised hydrochloric electrolytes is of great significance. In this research, proper oxidiser was introduced into pickling...

  • Polarographic Determination of Voriconazole in Pharmaceutical Formulations. Corbinia, Gianfranco; Zanfini, Assunta; La Rosa, Caterina; D'Arpino, Alessandro; Meucci, Rachele; Dreassi, Elena // Current Analytical Chemistry;Jul2009, Vol. 5 Issue 3, p238 

    This paper describes a method for voriconazole assay in pharmaceuticals by using differential pulse polarography (DPP). The voriconazole standard was obtained from pharmaceutical formulations and its purity determined by LC/UV, LC/ESI/MS and DSC analyses. In the DPP analysis a well defined peak...

  • Tungstate sharpening: A versatile method for extending the profile of ultra sharp tungsten probes. Stone, R.; Rosamond, M.; Coleman, K.; Petty, M.; Kolosov, O.; Bowen, L.; Dubrovskii, V.; Zeze, D. // Review of Scientific Instruments;Mar2013, Vol. 84 Issue 3, p035107 

    The benefits of a new electrochemical etching method for the controlled sharpening of sub-micron tungsten probes are demonstrated. The proposed technique only utilizes the insulating effect of the WO42- by-product which offers more practical ways of controlling the process parameters. The...

  • Relaxation mechanism in silver borate glasses. S. Yawale; V. Kharche // Glass Physics & Chemistry;Aug2008, Vol. 34 Issue 4, p381 

    Abstract  The electrical properties of silver ion conducting borate glasses are investigated by impedance spectroscopy in the temperature range 303–453 K. Impedance data are presented in the Nyquist plots. This representation allows the determination of the relaxation frequencies of...

  • Cyclic Voltammetric Studies of Carbon Steel in Deaerated NaHCO3 Solution. El-Naggar, M.M. // Journal of Applied Electrochemistry;Sep2004, Vol. 34 Issue 9, p911 

    The voltammetric response of per-cathodic activated carbon steel electrode in deaerated 0.50 m NaHCO3 solution at pH 8.72 and 25 °C at a scan rate of 25 mV s-1 was investigated. The influence of cycling, potential excursion and scanning rate on the anodic behavior was studied. The results...

  • Electrochemical studies on nanofiller incorporated poly(vinylidene fluoride–hexafluoropropylene) (PVdF–HFP) composite electrolytes for lithium batteries. Stephan, A. Manuel; Nahm, Kee Suk; Kulandainathan, M. Anbu; Ravi, G.; Wilson, J. // Journal of Applied Electrochemistry;Oct2006, Vol. 36 Issue 10, p1091 

    Composite polymer electrolytes (CPE), comprising poly(vinylidene fluoride-hexafluoropropylene) (PVdF-HFP), aluminum oxyhydroxide, (AlO[OH]n - of 40 nm and 7 pm) as filler and LiN(C2F5SO2)2 or LiClO4 as lithium salt were prepared using a solution casting technique. The membranes were subjected to...

  • Voltammetry in the scientific activities of I.P. Alimarin. Salikhdzhanova, R. M.-F.; Davletchin, D. I. // Journal of Analytical Chemistry;Sep2006, Vol. 61 Issue 9, p922 

    I.P. Alimarin was a pioneer in implementing voltammetry in our country. He contributed to the development of the practical application of the technique to the analysis of materials, ores, and rocks and investigated the potential of the technique in the determination of ultratrace concentrations...

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics