TITLE

A longitudinal-longitudinal mode TERFENOL-D/Pb(Mg1/3Nb2/3)O3–PbTiO3 laminate composite

AUTHOR(S)
Shuxiang Dong; Jie-Fang Li; Viehland, D.
PUB. DATE
November 2004
SOURCE
Applied Physics Letters;11/29/2004, Vol. 85 Issue 22, p5305
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
We have found that laminates of longitudinally magnetized magnetostrictive TERFENOL-D layersand a longitudinally poled piezoelectric Pb(Mg1/3Nb2/3)O3-PbTiO3 crystal have a giant magnetoelectric voltage coefficient of >430 mV/Oe under a low magnetic bias. Under a resonant drive operation at a frequency of 82.1 kHz, the magnetoelectric coefficient was dramatically increased to ∼18.5 V/Oe. In addition, an ultrahigh magnetic field sensitivity of <10-11 T has been observed.
ACCESSION #
15244137

 

Related Articles

  • Vortex magnetic field sensor based on ring-type magnetoelectric laminate. Shuxiang Dong; Jie-Fang Li; Viehland, D. // Applied Physics Letters;9/20/2004, Vol. 85 Issue 12, p2307 

    It has been found that ring-type magnetoelectric laminate composites of circumferentially magnetized magnetostrictive TERFENOL-D and a circumferentially poled piezoelectric Pb(Zr,Ti)O3 have high sensitivity to a vortex magnetic field. At room temperature, an induced output voltage from this ring...

  • Which Ply First? Pfund, Bruce // Professional Boatbuilder;Jun/Jul2007, Issue 107, p70 

    The article discusses ply sequencing and laminate repair in boats. It examines what occurs at the intersection of original construction and repair laminates. According to the experts the author consulted, fiber continuity and ply-to-ply correspondence are not that important to successful repair....

  • Bending of Laminated Composite Plates. Rakočević, Marina; Vatin, Nikolay // Applied Mechanics & Materials;2014, Vol. 740, p667 

    In this work, there are presented overviews of theoretical and numerical models for defining the stress-strain state in the cross section of moderately thick and thick composite plates in case of bending. Layered composite plates are constructed by combination of layers of various materials and...

  • Magnetoelectric sensor with miniature universal tunable bias magnetic circuit. Shi, Zhan; Tong, Yongshuai; Deng, Shuwen; Xue, Hao; Yang, Shuiyuan; Lu, Yong; Wang, Cuiping; Liu, Xingjun // Applied Physics Letters;7/15/2013, Vol. 103 Issue 3, p032903 

    This paper presents a miniature alternating magnetic field sensor made from magnetoelectric (ME) laminated materials with a universal tunable bias magnetic circuit. By adjusting the width of the bypass passage in the bias magnetic circuit, the magnetic flux in the ME materials could be tuned and...

  • Magnetoelectric performance of cylindrical Ni-lead zirconate titanate-Ni laminated composite synthesized by electroless deposition. Wu, W.; Bi, K.; Wang, Y. G. // Journal of Materials Science;Mar2011, Vol. 46 Issue 6, p1602 

    The cylindrical Ni-lead zirconate titanate (PZT)-Ni laminated composites with various magnetostrictive-piezoelectric phase thickness ratios were synthesized by electroless deposition. The influences of the bias magnetic field ( H) and the ac magnetic field frequency ( f) on magnetoelectric (ME)...

  • The new Steel-CFRP composite specimen (CFRP laminates sandwiched between two steel strips) and its behaviour under Uniaxial tension. Jawad Uriayer, Faris Abbas // International Journal of Civil & Structural Engineering;2012, Vol. 3 Issue 1, p249 

    This paper introduces new specimen of steel-Carbon Fibre Reinforce Polymer (CFRP) composite developed in accordance with standard test method and definition for mechanical testing of steel (ASTM -A370). Fifteen specimens were prepared and divided into five groups depending upon a number of the...

  • Enhanced coercivity in thermally processed (Nd,Dy)(Fe,Co,Nb,B)5.5/α-Fe nanoscale multilayer magnets. Liu, W.; Li, X. Z.; Liu, J. P.; Sun, X. K.; Chen, C. L.; Skomski, R.; Zhang, Z. D.; Sellmyer, D. J. // Journal of Applied Physics;5/15/2005, Vol. 97 Issue 10, p10R501 

    Structural and magnetic properties of laminated (Nd,Dy)(Fe,Co,Nb,B)5.5/Fe nanocomposites are investigated. Normally, the addition of the soft phase to the hard phase enhances the remanence but deteriorates the permanent-magnet performance of the material by reducing the coercivity. In the...

  • Myth.  // Printing World;Mar2008, p16 

    The article provides information about the characteristics, benefits and durability of films in printing industry. Since films used for over-print lamination are made from polypropylene, laminating can never be considered a green option. It has been mentioned that polypropylene is an oil...

  • Myth debunked.  // Printing World;Mar2008, p16 

    The article offers practical tips and cost-effectiveness of lamination. It protects a product and increases its life span, thereby saving on paper and materials. In addition, single-sided laminated sheets can still be sent for recycling in the normal manner as the film can be separated out...

Share

Read the Article

Courtesy of VIRGINIA BEACH PUBLIC LIBRARY AND SYSTEM

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics