ABSTRACT
The present study deals with the participation of fluid phases in the mechanochemical synthesis of phthalylsulphathiazole. Model experiments with optical microscope using crystalline samples revealed the possibility of the interaction between sulphathiazole and phthalic anhydride without their direct contact with each other at a temperature of about 100°C. The shift of the reaction temperature into lower-temperature region under mechanical activation of the reagents is demonstrated by means of scanning calorimetry. Assumption concerning the transport of phthalic anhydride through the gas phase as the most probable mechanism of synthesis in the mechanochemical reactor is put forward.
ACCESSION #
14360468

 

Related Articles

  • Mechanical alloying of Fe-transition metal systems: The analysis of different stages. Povstugar, L. V.; Butyagin, P. Yu. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5461 

    The paper presents the results of the quantitative analysis of mechanical alloying (MA) in binary systems Fe-X (X = Ti, Zr, Nb, Mo, Ta, W). MA has been studied as a sequence of interrelated microscopic processes (structural refinement of initial components, consumption of Fe and X, transition of...

  • Effect of the ball mass to sample mass relation in the magnetic and structural properties of Fe0.6Mn0.1Al0.3 alloys prepared by mechanical alloying. Valderruten, J. F.; Alcázar, G. A. Pérez; Civale, L. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5445 

    Fe0.6Mn0.1Al0.3 samples were prepared by mechanical alloying (MA) using the 6:1, 9:1 and 12:1 ratios between the ball mass and powder mass (BM/PM) and milling times of 3, 6, 9 and 12 h. Balls of 10 and 20 mm diameter were used. X-ray diffraction (XRD) studies showed that the 6:1 and 9:1 samples...

  • Mechanochemically assisted synthesis of FeVO4 catalysts. Klissurski, D.; Iordanova, R.; Radev, D.; Kassabov, St.; Milanova, M.; Chakarova, K. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5375 

    The influence of mechanochemical treatment on the solid state reactions between α-Fe2O3 and V2O5 was studied. A stoichiometric mixture of both oxides was subjected to an intense milling in air for different time intervals. The mechanochemical treatment for 15 h leads to a drastic decrease of...

  • Nanosized mechanocomposites and solid solution in immiscible metal systems. Lyakhov, N.; Grigorieva, T.; Barinova, A.; Lomayeva, S.; Yelsukov, E.; Ulyanov, A. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5421 

    Mechanical alloying is the most perspective method for preparation of nanosized mechanocomposites in non-mixed liquid and solid metals. It is known that plastic metals get fragile in the presence of the liquid metal phase, and this phase spreads over the surface of solid metal due to good...

  • Application of AFM to study functional nanomaterials prepared by mechanical alloying. Jakubowicz, J. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5379 

    Two-phase hard magnetic Nd2Fe14B/α-Fe nanocomposites and nanocrystalline TiFe electrode materials were prepared by mechanical alloying and heat treatment. The microstructure of both types of functional nanomaterials was investigated by atomic force microscopy. In the case of Nd2Fe14B magnetic...

  • Mechanochemical synthesis of SnO-B2O3 glassy anode materials for rechargeable lithium batteries. Hayashi, A.; Nakai, M.; Morimoto, H.; Minami, T.; Tatsumisago, M. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5361 

    The xSnO·(100 - x)B2O3 (0 ≦ x ≦ 80) glasses were successfully prepared by a mechanical milling technique. The glass with 40 mol% SnO showed the maximum glass transition temperature of 347°C. The SnO-B2O3 milled glasses consisted of both BO3 and BO4 units, and the fraction of...

  • Direct formation of Na3AlH6 by mechanical milling NaH/Al with TiF3. Wang, P.; Kang, X. D.; Cheng, H. M. // Applied Physics Letters;8/15/2005, Vol. 87 Issue 7, p071911 

    Na3AlH6 can be directly formed by mechanical milling NaH/Al with TiF3 under hydrogen atmosphere. The hydrogenation fraction of NaH increases with increasing the milling time, and reaches up to 0.61 after 20 h milling. Thus-formed Na3AlH6 exhibits unexpected polymorphic transformation and...

  • Mechanochemical synthesis of nano-sized Bi2V0.9CU0.1O5.35 powders. Zhang, T. S.; Ma, J.; Kong, L. B. // Journal of Materials Research;Jan2006, Vol. 21 Issue 1, p71 

    Nano-sized Bi2V0.9CU0.1O5.35 powders were synthesized via a mechanochemical route from the component oxide mixture. However, a ball-milling duration of over 30 h was needed to ensure a high phase purity. Otherwise, the milled samples had poor sinterability and low sintered density since...

  • On the analysis of mechanism of supersaturation of metal powders with interstitial impurities during mechanical activation. Vasil'ev, L. S.; Lomayeva, S. F. // Journal of Materials Science;Aug2004, Vol. 39 Issue 16/17, p5411 

    The paper discusses the mechanisms of formation of nanostructure, chemical and phase composition, and dispersity of the particles of metal powders obtained in the process of mechanochemical activation and of mechanical alloying. It has been shown that the processes of plastic deformation and...

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics