TITLE

Comment on “A critical examination of the P–h2 relationship in nanoindentation” [Appl. Phys. Lett. 83, 863 (2003)]

AUTHOR(S)
Malzbender, Jürgen
PUB. DATE
June 2004
SOURCE
Applied Physics Letters;6/7/2004, Vol. 84 Issue 23, p4813
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
Comments on the article "A critical examination of the P—h2 relationship in nanoindentation" published in the volume 83, 2003 issue of the periodical "Applied Physics Letter." Attempts of the author to extend a load-displacement relationship; Dependency of the geometric constant on the power law exponent of the unloading curve; Questions on the validity of expression for elasto-plastic indentation.
ACCESSION #
13203681

 

Related Articles

  • A GEOMETRIC REPRESENTATION OF THE SUM OF FOURTH POWERS OF POSITIVE INTEGERS. Chilaka, James O. // Mathematics & Computer Education;Winter2005, Vol. 39 Issue 1, p69 

    Presents a geometric representation of the sum of the fourth powers of positive integers. Formula for sum of fourth powers of positive integers; Sum of squares of triangular numbers.

  • Response to “Comment on ‘A critical examination of the P–h2 relationship in nanoindentation’ ” [Appl. Phys. Lett. 84, 4813 (2004)]. Troyon, Michel // Applied Physics Letters;6/7/2004, Vol. 84 Issue 23, p4814 

    Presents a response to a comment on the article "A Critical Examination of the P-h2 Relationship in Nanoindentation." Definition of an axisymmetric punch as a function of the power law exponent of the unloading curve; Consequences of the complex elastic/plastic deformation occuring at the...

  • Search Space Pruning to Solve the Root Identification Problem in Geometric Constraint Solving. Joan-Arinyo, R.; Luzón, M. V.; Yeguas, E. // Computer-Aided Design & Applications;2009, Vol. 6 Issue 1, p15 

    Geometric constraint solving is at the core of parametric computer-aided geometric design where the main issue is selecting a given solution among a potentially exponential number of solution instances in the number of geometric elements involved in the geometric model. Since the user is only...

  • GEOMETRIC AND TOPOLOGICAL PROPERTIES OF EXPONENT RELATED DYNAMIC EVOLUTION. XIN YANG LU // Communications in Mathematical Analysis;2012, Vol. 12 Issue 2, p102 

    In this paper we consider the discrete dynamic evolution of a connected network related to an average distance functional minimization problem, with associated dissipation term, under irreversibility assumption. We will analyze its geometric and topological properties, and study whether it...

  • ON SOME APPLICATIONS OF FINITE GALOIS STABLE LINEAR GROUPS. Khrebtova, Ekaterina; Malinin, Dmitry // Proceedings of World Academy of Science: Engineering & Technolog; 

    We consider a Galois extensions E/F and realization fields of finite abelian subgroups G ⊂ GLn(E) of a given exponent t. Let us assume that G is stable under the natural operation of the Galois group of E/F. It is proven that under some reasonable restrictions for n any E can be a...

  • Errata.  // Operations Research;Jul/Aug83, Vol. 31 Issue 4, p802 

    Presents corrections to the article "Beta Variate Generation via Exponential Majorizing Functions," by B. W. Schmeiser and A. J. G. Babu, published in the February 1983 issue.

  • Horsefeathers. Coontz Jr., Robert J. // Sciences;Nov/Dec94, Vol. 34 Issue 6, p12 

    Presents prefixes used in the description of numerical quantity. Etymology of the prefixes; History of the usage of the prefixes; List of prefixes used to describe the exponential power of base ten system of counting.

  • Powers Struggle! Friedman, Matt // Scholastic Math;10/11/2004, Vol. 25 Issue 3, p14 

    Presents a quiz on exponents.

  • Exponents in the House! D'Amico, Cara // Scholastic Math;10/9/2006, Vol. 27 Issue 3, p16 

    A quiz regarding exponents is presented.

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics