Mechanical response of KD[sub 2x]H[sub 2(1-x)]PO[sub 4] crystals during nanoindentation

AUTHOR(S)
Kucheyev, S.O.; Siekhaus, W.J.; Land, T.A.; Demos, S.G.
PUB. DATE
March 2004
SOURCE
Applied Physics Letters;3/29/2004, Vol. 84 Issue 13, p2274
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
The deformation behavior of rapidly grown tetragonal KD[sub 2x]H[sub 2(1-x)]PO[sub 4] (KDP and DKDP) single crystals, with a deuteration degree x of 0.0, 0.3, and 0.6, is studied by nanoindentation with a 1 μm radius spherical indenter. Within experimental error, the deformation behavior is found to be independent of the deuterium content and different for (001) and (100) surfaces. Multiple discontinuities (so-called “pop-in” events) in force-displacement curves are observed during indentation loading, but not during unloading. Slip is identified as the major mode of plastic deformation in DKDP, and pop-in events are attributed to the initiation of slip. © 2004 American Institute of Physics.
ACCESSION #
12606875

 

Related Articles

  • Study on the interaction between a dislocation and impurities in KCl:Sr2+ single crystals by the Blaha effect Part III Influence of heat treatment on various characteristics. Kohzuki, Y.; Ohgaku, T. // Journal of Materials Science;Jan2004, Vol. 39 Issue 1, p107 

    Strain-rate cycling tests associated with ultrasonic oscillation were conducted at 80�239 K for two kinds of KCl:Sr2+ (0.05 mol% in the melt) single crystals: quenched and annealed specimens. Examining the relationship of temperature and dislocation velocity-effective stress exponent, m*,...

  • Hardening of Crystals Caused by the Dynamic Aging of Dislocations. Petukhov, B.V. // Crystallography Reports;Sep2003, Vol. 48 Issue 5, p813 

    A model relating the pronounced effect of mobile impurities on the processes of plastic deformation in crystals to the dynamic aging of dislocations is proposed. The model is based on the concept of internal stresses depending individually on the age of dislocations due to the difference in the...

  • Disorientation relations during the early stages of recrystallization in medium and low SFE fee metals. Miszczyk, M.; Paul, H.; Driver, J. H.; Maurice, C. // Materials Science Forum;2014, Vol. 783-786, p2585 

    The objective of this paper is to identify the predominant crystallographic relations between deformed state and recrystallized grains during the early stages of recrystallization of fee metals with medium and low stacking fault energy. The experimental investigations, based on SEM/EBSD...

  • Phase transformation and nanograin refinement of silicon by processing through high-pressure torsion. Ikoma, Yoshifumi; Hayano, Kazunori; Edalati, Kaveh; Saito, Katsuhiko; Guo, Qixin; Horita, Zenji // Applied Physics Letters;9/17/2012, Vol. 101 Issue 12, p121908 

    Si(100) wafers were subjected to severe plastic deformation under a pressure of 24 GPa using high-pressure torsion (HPT). Si wafers were plastically deformed at room temperature. HPT-processed samples were composed of metastable body centered cubic Si-III and rhombohedral Si-XII phases in the...

  • DISLOCATION MECHANICS OF IRON AND COPPER IN HIGH RATE DEFORMATION TESTS. Armstrong, Ronald W.; Arnold, Werner; Zerilli, Frank J. // AIP Conference Proceedings;12/28/2009, Vol. 1195 Issue 1, p1105 

    For shocked iron, there is competition between grain size dependent slip or deformation twinning responses at the Hugoniot elastic limit (HEL) while, at higher stress, there is predicted control of the shock-induced plastic strain rate by the grain size independent generation at the propagating...

  • Liquid crystal helical ribbons as isometric textures. Achard, M.-F.; Kleman, M.; Nastishin, Yu. A.; Nguyen, H.-T. // European Physical Journal E -- Soft Matter;Jan2005, Vol. 16 Issue 1, p37 

    Deformations that conserve the parallelism and the distances - between layers, in smectic phases; between columns, in columnar phases - are commonplace in liquid crystals. The resulting isometric deformed textures display specific geometric features. The corresponding order parameter...

  • Deformation at the contacts of sodium chloride crystals in the presence of water. Skvortsova, Z.N.; Kas’yanova, I.V.; Porodenko, E.V.; Traskine, V.Yu. // Colloid Journal;Sep2007, Vol. 69 Issue 5, p643 

    The processes taking place at the intergrain contacts during powder pressing in dissolving media are studied. The threshold stress corresponding to a change in the mechanism (the transition from the dislocation glide to the recrystallization creep) of sodium chloride deformation in the presence...

  • Local heating and quasiathermal plastic deformation of crystals at low temperatures. Malygin, G. A. // Physics of the Solid State;Nov97, Vol. 39 Issue 11, p1806 

    A theoretical discussion is given of the relationship between local heating of a crystal by glide lines and bands and deviations observed in the temperature dependences of the flow stresses and their rate coefficients at low temperatures (< 10 K) from the dependences characteristic of thermally...

  • Dynamic blocking of the influence of surface point defects on the glide of edge dislocations. Malashenko, V. V. // Physics of the Solid State;Apr2009, Vol. 51 Issue 4, p744 

    The influence of image forces on an edge dislocation gliding parallel to the free crystal surface having point defects is studied theoretically. It is shown that image forces block the drag mechanism that involves the excitation of dislocation vibrations by surface defects.

Share

Read the Article

Courtesy of VIRGINIA BEACH PUBLIC LIBRARY AND SYSTEM

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics