This paper uses micro-grinding tool with 500# grains and 0.9 mm diameter to grind nickel-based superalloy Inconel600 through three factors(grinding depth, feed rate, spindle speed ) at three levels orthogonal grinding experiment in mesoscopic scale. Then according to the range analysis of surface roughness, the primary and secondary influencial factors are found; the micro grinding parameters are optimized,the results show: the influence of the feed rate(vf )is the biggest, followed by the spindle speed(n), the grinding depth(ap) is minimal, when n=50kr/min, vf=100µm/s, ap =6µm, the grinding surface roughness is minimum: Ra =579nm; finally, the regression mathematical model of micro grinding surface roughness is established, the relative error of the calculated value and experimental measurements is low, showing that this regression mathematical model is accurate and effective. This study provides a theoretical basis for the micro grinding parameters and surface quality control of nickel-based superally.
ACCESSION #
110788012

 

Related Articles

  • Experiment and Surface Roughness Prediction Model for Ti-6Al-4V in Abrasive Belt Grinding. Yaxiong Chen; Yun Huang; Guijian Xiao; Guilin Chen; Zhiwu Liu; Xiumei Liu // Advanced Materials Research;2015, Vol. 806, p42 

    In abrasive belt grinding, abrasive belt granularity, abrasive belt speed, feeding speed and grinding force have a great influence on the surface roughness. In order to predicate the surface roughness of Ti-6Al-4V,a response surface methodology are used to build the model to predict surface...

  • Surface roughness and topography of honed nickel-based superalloy. YANG Changyong; FU Yucan; HUANG Dashun; XU Jiuhua; YANG Nengge; YAN Wen // Advanced Materials Research;2015, Vol. 806, p478 

    Honing experiments were carried out for nickel-based superalloy Inconel718 bore. The significance analysis of the four honing parameters: spindle speed, stroke speed, wedge feed per stroke cycle and grain size on the surface roughness, was studied with the orthogonal design method. And the...

  • Experimental investigation on the electrochemical machining of 00Cr12Ni9Mo4Cu2 material and multi-objective parameters optimization. Tang, L.; Yang, S. // International Journal of Advanced Manufacturing Technology;Aug2013, Vol. 67 Issue 9-12, p2909 

    Special stainless steel 00Cr12Ni9Mo4Cu2 has multiple composition and inhomogeneous tissues; short circuiting will frequently occur when using conventional electrolyte processing. This article analyzes the reason why the process of machining is difficult from the material composition and...

  • Surface roughness and topography of honed nickel-based superalloy. YANG Changyong; FU Yucan; HUANG Dashun; XU Jiuhua; YANG Nengge; YAN Wen // Advanced Materials Research;2016, Vol. 1136, p478 

    Honing experiments were carried out for nickel-based superalloy Inconel718 bore. The significance analysis of the four honing parameters: spindle speed, stroke speed, wedge feed per stroke cycle and grain size on the surface roughness, was studied with the orthogonal design method. And the...

  • Experimental Study on the Surface roughness in Mesoscopic-scale Grinding of Nickel-based Superalloy. Zhou YunGuang; Gong YaDon; Sun Yang; Zhu ZongXiao; Gao Qi // Advanced Materials Research;2016, Vol. 1136, p9 

    This paper uses micro-grinding tool with 500# grains and 0.9 mm diameter to grind nickel-based superalloy Inconel600 through three factors(grinding depth, feed rate, spindle speed) at three levels orthogonal grinding experiment in mesoscopic scale. Then according to the range analysis of surface...

  • Experimental Study on Surface Quality in Micro-milling of Single Crystal Superalloy. GAO Qi; GONG Ya-dong; ZHOU Yun-guang // Advanced Materials Research;2016, Vol. 1136, p196 

    Single crystal Ni3Al-based superalloy has excellent comprehensive performance. To study the micro-milling surface quality of Ni3Al-based superalloy, this article used two-edged carbide alloy micro-milling tool with 0.8mm diameter, then orthogonal experiment of three factors and five levels was...

  • Deep Profiled Slot Grinding on a Nickel-based Alloy with Electroplated CBN Wheels. Zhongde Shi; Elfizy, Amr; Attia, Helmi // Advanced Materials Research;2015, Vol. 806, p3 

    A process for grinding deep profiled slots in a nickel-based alloy with electroplated cubic boron nitride (CBN) wheels and straight oil is presented. These slots were prepared by this process for further grinding with electroplated CBN quills to generate the final fir-tree slots in gas turbine...

  • Dressing Characteristics in Nitriding Treated Bearing Steel Under Ceramic Wheel Grinding Conditions. Sung Hoon Oh // International Journal of Control & Automation;Sep2012, Vol. 5 Issue 3, p133 

    In the grinding operation dressing sequence give proper profile and surface dimensions. Dressing eliminates loaded part in the wheel surface and makes wheel edge sharpening. Also specific surface profile in the dressing unit conveys to the material, and this is the main function with the...

  • Optimization of Surface Grinding Process Parameters for Minimum Surface Roughness in AISI 1080 Using Response Surface Methodology. Periyasamy, S.; Aravind, M.; Vivek, D.; Amirthagadeswaran, K. S. // Advanced Materials Research;2014, Vol. 984-985, p118 

    In this study, the response surface methodology was used to optimize the process parameters of constant speed horizontal spindle surface grinding. The experiments were conducted based on the design expert software. The surface roughness characteristics were investigated in AISI 1080 steel plates...

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics